Volfram agyr garyndy derejesi:
W90NiFe / W92.5NiFe / W93NiFe / W95NiFe / W97NiFe (Biraz Magnit).
W90NiCu / W92.5NiCu / W93NiCu / W95NiCu / W97NiCu (Magnit däl).
Dykyzlygy:16.8-18.8g / cm3.
Faceüzü:Işlenen we ýer.
Standart:ASTM B777.
Diametri:5.0mm - 80mm.
Uzynlyk:50mm - 350mm.
Dokary dykyzlyk (Gurşundan 65% dykyz).
Has dykyz materiallar bar (arassa volfram, altyn, platina topar metallary), ýöne olaryň ulanylmagy elýeterliligi, işlemegi we bahasy bilen çäklendirilýär.
Sesiň çäkli ýerinde köpçülik bilen üpjün etmek.
Massa ýerleşdirilende takyklyk zerur bolan konsentrirlenen agram.
Howa akymynyň ep-esli täsir edýän ýagdaýlarynda agramyň ýerleşdirilmegi.
Softokary ýumşadyjy temperatura.
Pes ýylylyk geçirijiligi we giňelişiň pes koeffisiýenti material termiki ýadawlyga ýokary garşylyk berýär.
Eredilen alýumine ajaýyp lehim eroziýa garşylygy.Highokary ýylylyk durnuklylygy bilen ýokary temperaturada güýçli.
Young Youngokary çeýeligiň moduly.Gurşundan tapawutlylykda möhüm güýçleri başdan geçireniňde süýrenmeýär.
Their Güýçlerine garamazdan, süýümli we ýarylmaga çydamly bolýarlar.
The Garyndylaryň gatylygy diapazony adatça 20-35 gatylyk HRC.
Garyndy görnüşi(%) | HD17 90W 6Ni 4Cu | HD17D 90W 7Ni 3Fe | HD17.5 92.5W 5.25Ni 2.25Fe | HD17.6 92.5W Balans Ni, Fe, Mo. | HD17.7 93W Balans Ni, Fe, Mo. | HD18 95W 3.5Ni 1.5Cu | HD18D 95W 3.5Ni 1.5Fe | HD18.5 97W 2.1Ni .9Fe |
MIL-T-21014 | 1-nji synp | 1-nji synp | 1-nji synp | - | - | 3-nji synp | 3-nji synp | 4-nji synp |
SAE-AMS-T-21014 | 1-nji synp | 1-nji synp | 2-nji synp | - | - | 3-nji synp | 3-nji synp | 4-nji synp |
AMS 7725 C. | 7725 C. | 7725 C. | -- | -- | -- | -- | -- | -- |
ASTM B777-87 | 1-nji synp | 1-nji synp | 2-nji synp | - | - | 3-nji synp | 3-nji synp | 4-nji synp |
Adaty dykyzlyk(g / cc) | 17.1 | 17.1 | 17.5 | 17.6 | 17.7 | 18 | 18 | 18.5 |
Adaty dykyzlyk(lbs / in3) | 0.614 | 0.614 | 0.632 | 0.636 | 0.639 | 0.65 | 0.65 | 0.668 |
Adaty gatylyk RC | 24 | 25 | 26 | 30 | 32 | 27 | 27 | 28 |
Ahyrky dartyş güýji min(ksi) | 110,000 | 120,000 | 114,000 | 120,000 | 125,000 | 110,000 | 120,000 | 123,000 |
0,2% hasyl bermegiň güýji min(ksi) | 80,000 | 88,000 | 84,000 | 90,000 | 95,000 | 85,000 | 90,000 | 85,000 |
Iň az% uzalma(1 "geýjiň uzynlygy) | 6 | 10 | 7 | 4 | 4 | 7 | 7 | 5 |
Proporsional elastik çäk(PSI) | 45,000 | 52,000 | 46,000 | 55,000 | 60,000 | 45,000 | 44,000 | 45,000 |
Çeýeligiň moduly(x106psi) | 40 x 106 | 45 x 106 | 47 x 106 | 52 x 106 | 53 x 106 | 45 x 106 | 50 x 106 | 53 x 106 |
Termiki giňeliş koeffisiýenti x10-6 / 0C(20-400C) | 5.4 | 4.61 | 4.62 | 4.5 | 4.5 | 4.43 | 4.6 | 4.5 |
Malylylyk geçirijiligi(CGS bölümleri) | 0.23 | 0.18 | 0.2 | 0.27 | 0.27 | 0.33 | 0.26 | 0.3 |
Elektrik geçirijiligi(% IACS) | 14 | 10 | 13 | 14 | 14 | 16 | 13 | 17 |
Magnit | No | Az salym | Az salym | Az salym | Az salym | No | Az salym | Az salym |